For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24345
Run/Test Number: L4239
Technique: Jiggered, dip-glazed, cast handle
Firing Schedule – C10RPL
Temperature – Cone 10R
Glaze Inside – G2571A Bamboo
Glaze Outside – G2571A bamboo matte
Clay Body – H550 Casting
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 94 mm (3.7 in)
Depth at rim (including handle) – 122 mm (4.8 in)
Height – 110 mm (4.3 in)
Weight – 428 grams (15.1 oz)
Registration Page: https://digitalfire.com/potterytony/2488