For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24360
Run/Test Number: L4484D
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.
Firing Schedule – PLC6DS
Temperature – Cone 6
Glaze Inside – G3914A
Glaze Outside – G3939A
Clay Body – L4484D MNP black
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 97 mm (3.8 in)
Depth at rim (including handle) – 130 mm (5.1 in)
Height – 116 mm (4.6 in)
Weight – 358 grams (12.6 oz)
Registration Page: https://digitalfire.com/potterytony/2502