Oatmeal glazed MNP black porcelain mug

$40.00

Oatmeal glazed MNP black porcelain mug

SKU: AJ24424 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24424
Run/Test Number: L4484D
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG3914A
Glaze OutsideG3939A
Clay BodyL4484D MNP black
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 99 mm (3.9 in)
Depth at rim (including handle) – 131 mm (5.2 in)
Height – 116 mm (4.6 in)
Weight – 360 grams (12.7 oz)

Registration Page: https://digitalfire.com/potterytony/2557

Weight 360 g
Dimensions 131.00 × 99.00 × 116.00 mm