For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24024
Run/Test Number: P6847
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – C10RPL
Temperature – Cone 10R
Glaze Inside – G1947U
Glaze Outside – G2571D
Clay Body – H570
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 100 mm (3.9 in)
Depth at rim (including handle) – 127 mm (5.0 in)
Height – 130 mm (5.1 in)
Weight – 373 grams (13.1 oz)
Registration Page: https://digitalfire.com/potterytony/2382