Serial Number: AJ24027
Run/Test Number: P6816
Technique: Thrown, engobed, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – C10RPL
Temperature – Cone 10R
Glaze Inside – G1947U
Glaze Outside – GR10-C
Engobe – L3954N
Clay Body – H550
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 102 mm (4.0 in)
Depth at rim (including handle) – 130 mm (5.1 in)
Height – 122 mm (4.8 in)
Weight – 433 grams (15.3 oz)