For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24427
Run/Test Number: P7027
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – C6DHSC
Temperature – Cone 6
Glaze Inside – G3914A
Glaze Outside – G2934Y Red
Clay Body – M370
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 93 mm (3.7 in)
Depth at rim (including handle) – 122 mm (4.8 in)
Height – 113 mm (4.4 in)
Weight – 356 grams (12.5 oz)
Registration Page: https://digitalfire.com/potterytony/2560