Reduction fired buff stoneware deep blue mug

$35.00

H550 compatible clay body made from Blue Hills and FlintOft, SK clays.

SKU: AJ24326 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24326
Run/Test Number: L4380A
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed
Description: H550 compatible clay body made from Blue Hills and FlintOft, SK clays.

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideG2571F
Glaze OutsideG2571F
EngobeL3954N
Clay BodyH550 Test
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 96 mm (3.8 in)
Depth at rim (including handle) – 128 mm (5.0 in)
Height – 111 mm (4.4 in)
Weight – 353 grams (12.4 oz)

Registration Page: https://digitalfire.com/potterytony/2470

Weight 353 g
Dimensions 128.00 × 96.00 × 111.00 mm