For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24157
Run/Test Number: P6823
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – C6DHSC
Temperature – Cone 6
Glaze Inside – L3500G+2Fe
Glaze Outside – GA6-C
Clay Body – M350
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 95 mm (3.7 in)
Depth at rim (including handle) – 125 mm (4.9 in)
Height – 119 mm (4.7 in)
Weight – 367 grams (12.9 oz)
Registration Page: https://digitalfire.com/potterytony/2399