Rutile blue brown stoneware mug

$35.00

Rutile blue brown stoneware mug

SKU: AJ24077 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24077
Run/Test Number: P6823
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze Inside – L3500G+2Fe
Glaze OutsideGA6-C
Clay BodyM350
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 100 mm (3.9 in)
Depth at rim (including handle) – 129 mm (5.1 in)
Height – 116 mm (4.6 in)
Weight – 431 grams (15.2 oz)

Registration Page: https://digitalfire.com/potterytony/2414