Rutile blue buff stoneware mug

$35.00

Rutile blue buff stoneware mug

SKU: AJ24084 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24084
Run/Test Number: L4212
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideGA6-C
Glaze Outside – GA6-C
EngobeL3954B
Clay BodyM340
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 96 mm (3.8 in)
Depth at rim (including handle) – 130 mm (5.1 in)
Height – 115 mm (4.5 in)
Weight – 421 grams (14.8 oz)

Registration Page: https://digitalfire.com/potterytony/2428

Weight 421 g
Dimensions 130.00 × 96.00 × 115.00 mm