Rutile blue buff stoneware mug

$35.00

Rutile blue buff stoneware mug

SKU: AJ24102 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24102
Run/Test Number: P6770
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideGA6-C
Glaze Outside – GA6-C
EngobeL3954B
Clay BodyM340
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 102 mm (4.0 in)
Depth at rim (including handle) – 133 mm (5.2 in)
Height – 121 mm (4.8 in)
Weight – 459 grams (16.2 oz)

Registration Page: https://digitalfire.com/potterytony/2429

Weight 459 g
Dimensions 133.00 × 102.00 × 121.00 mm