Satin blue MNS stoneware mug

$40.00

Satin blue MNS stoneware mug

SKU: AJ24384 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24384
Run/Test Number: L4249C
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideG2934Y Blue
Clay Body – L4249C MNS
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 92 mm (3.6 in)
Depth at rim (including handle) – 124 mm (4.9 in)
Height – 98 mm (3.9 in)
Weight – 349 grams (12.3 oz)

Registration Page: https://digitalfire.com/potterytony/2520

Weight 349 g
Dimensions 124.00 × 92.00 × 98.00 mm