Run/Test Number: P6806
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideG2934Y Yellow
Clay BodyPolar Ice
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 91 mm (3.6 in)
Depth at rim (including handle) – 122 mm (4.8 in)
Height – 114 mm (4.5 in)
Weight – 328 grams (11.6 oz)

Registration Page: https://digitalfire.com/potterytony/2420

Weight 328 g