Translucent Polar Ice porcelain mug

$35.00

Translucent Polar Ice porcelain mug

SKU: AJ24049 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24049
Run/Test Number: P6803
Technique: Thrown, incised, dip-glazed

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideG2926B
Clay BodyPolar Ice
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 96 mm (3.8 in)
Depth at rim (including handle) – 131 mm (5.2 in)
Height – 108 mm (4.3 in)
Weight – 354 grams (12.5 oz)

Registration Page: https://digitalfire.com/potterytony/2359

Weight 354 g
Dimensions 131.00 × 96.00 × 108.00 mm