Serial Number: AJ24386
Run/Test Number: P7004
Technique: Thrown, transfers applied at leather hard, liner-glazed inside, dip-glazed outside
Firing Schedule – C6DHSC
Temperature – Cone 6
Glaze Inside – G2934 Red
Glaze Outside – G2934
Clay Body – M370
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 95 mm (3.7 in)
Depth at rim (including handle) – 128 mm (5.0 in)
Height – 110 mm (4.3 in)
Weight – 341 grams (12.0 oz)