For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24105
Run/Test Number: P6729
Technique: Thrown, incised, dip-glazed
Firing Schedule – PLC6DS
Temperature – Cone 6
Glaze Inside – GR6-M
Glaze Outside – GR6-M
Clay Body – Coffee Clay
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 95 mm (3.7 in)
Depth at rim (including handle) – 128 mm (5.0 in)
Height – 124 mm (4.9 in)
Weight – 345 grams (12.2 oz)