For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24439
Run/Test Number: L4471J2
Technique: Thrown, incised, dip-glazed
Firing Schedule – PLC6DS
Temperature – Cone 6
Glaze Inside – G3926B
Glaze Outside – G3926B
Clay Body – M340S
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 95 mm (3.7 in)
Depth at rim (including handle) – 131 mm (5.2 in)
Height – 122 mm (4.8 in)
Weight – 369 grams (13.0 oz)
Registration Page: https://digitalfire.com/potterytony/2572