White glossy glazed reduction fired mug

$45.00

White glossy glazed reduction fired mug

SKU: AJ24422 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24422
Run/Test Number: L4453E
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideG1947U
Glaze OutsideGR10-CW
Clay BodyH550
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 95 mm (3.7 in)
Depth at rim (including handle) – 132 mm (5.2 in)
Height – 108 mm (4.3 in)
Weight – 350 grams (12.3 oz)

Registration Page: https://digitalfire.com/potterytony/2555

Weight 350 g
Dimensions 132.00 × 95.00 × 108.00 mm