For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24423
Run/Test Number: L4453E
Technique: Thrown, incised, dip-glazed
Firing Schedule – C10RPL
Temperature – Cone 10R
Glaze Inside – GR10-A
Glaze Outside – GR10-A
Clay Body – H550
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 100 mm (3.9 in)
Depth at rim (including handle) – 128 mm (5.0 in)
Height – 117 mm (4.6 in)
Weight – 395 grams (13.9 oz)
Registration Page: https://digitalfire.com/potterytony/2556