Zero3 fritware porcelain hash-tag mug

$40.00

Zero3 fritware porcelain hash-tag mug

SKU: AJ24137 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24137
Run/Test Number: L3924C
Technique: Thrown, leather-hard under-glaze decorated, incised, 1650F bisque fired, dip-glazed

Firing ScheduleC04PLTP
Temperature – Cone 03
Glaze InsideG2931K
Glaze OutsideG2931K
Clay BodyL3924C
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 85 mm (3.3 in)
Depth at rim (including handle) – 118 mm (4.6 in)
Height – 122 mm (4.8 in)
Weight – 339 grams (11.9 oz)

Registration Page: https://digitalfire.com/potterytony/2275

Weight 339 g
Dimensions 118.00 × 85.00 × 122.00 mm