Copper blue-green Grolleg porcelain mug

$40.00

Copper blue-green Grolleg porcelain mug

SKU: AJ24018 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24018
Run/Test Number: L3778D
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideG3806E
Clay BodyL3778D
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 89 mm (3.5 in)
Depth at rim (including handle) – 117 mm (4.6 in)
Height – 101 mm (4.0 in)
Weight – 194 grams (6.8 oz)

Registration Page: https://digitalfire.com/potterytony/2376

Weight 194 g
Dimensions 117.00 × 89.00 × 101.00 mm