Copper blue-green Crysanthos porcelain mug

$40.00

Copper blue-green Crysanthos porcelain mug

SKU: AJ240210 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ240210
Run/Test Number: L3611A
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideG3806E
Clay Body – L3611A
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 87 mm (3.4 in)
Depth at rim (including handle) – 119 mm (4.7 in)
Height – 99 mm (3.9 in)
Weight – 329 grams (11.6 oz)

Registration Page: https://digitalfire.com/potterytony/2375

Weight 329 g
Dimensions 119.00 × 87.00 × 99.00 mm