Rutile blue black Coffee Clay stoneware mug

$40.00

Rutile blue black Coffee Clay stoneware mug

SKU: AJ24010 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24010
Run/Test Number: P6831
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideGA6-B
Glaze Outside – GA6-C
Clay Body – Coffee
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 94 mm (3.7 in)
Depth at rim (including handle) – 128 mm (5.0 in)
Height – 109 mm (4.3 in)
Weight – 362 grams (12.8 oz)

Registration Page: https://digitalfire.com/potterytony/2367

Weight 362 g
Dimensions 128.00 × 94.00 × 109.00 mm