Copper blue-green M370 porcelain mug

$40.00

Copper blue-green M370 porcelain mug

SKU: AJ24020 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24020
Run/Test Number: P6848
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideG3806E
Clay BodyM370
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 95 mm (3.7 in)
Depth at rim (including handle) – 122 mm (4.8 in)
Height – 115 mm (4.5 in)
Weight – 357 grams (12.6 oz)

Registration Page: https://digitalfire.com/potterytony/2374

Weight 357 g