Serial Number: AJ24139
Run/Test Number: P6699
Technique: Hand-rolled, embossed and assembled, liner-glazed inside, dip-glazed outside
Firing Schedule – C10RPL
Temperature – Cone 10R
Glaze Inside – G1947U
Glaze Outside – G2571A
Engobe – L3954N
Clay Body – H570
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 96 mm (3.8 in)
Depth at rim (including handle) – 123 mm (4.8 in)
Height – 102 mm (4.0 in)
Weight – 327 grams (11.5 oz)