Serial Number: AJ24156
Run/Test Number: P6823
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze Inside – L3500G+2Fe
Glaze OutsideGA6-C
Clay BodyM350
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 102 mm (4.0 in)
Depth at rim (including handle) – 130 mm (5.1 in)
Height – 121 mm (4.8 in)
Weight – 469 grams (16.5 oz)

Registration Page: https://digitalfire.com/potterytony/2398