Blue Porcelain Mug

$45.00

Blue Porcelain Mug

SKU: AJ24100 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24100
Run/Test Number: P6746
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideG2934Y Blue
Clay BodyM370
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 92 mm (3.6 in)
Depth at rim (including handle) – 120 mm (4.7 in)
Height – 105 mm (4.1 in)
Weight – 382 grams (13.5 oz)

Registration Page: https://digitalfire.com/potterytony/2417

Weight 382 g
Dimensions 120.00 × 92.00 × 105.00 mm