Translucent Polar Ice porcelain reduction-fired mug

$35.00

Translucent Polar Ice porcelain reduction-fired mug

SKU: AJ24154 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24154
Run/Test Number: L3875C
Technique: Thrown, incised, dip-glazed

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideG1947U
Glaze OutsideG1947U
Clay BodyPolar Ice
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 93 mm (3.7 in)
Depth at rim (including handle) – 126 mm (5.0 in)
Height – 112 mm (4.4 in)
Weight – 328 grams (11.6 oz)

Registration Page: https://digitalfire.com/potterytony/2347

Weight 328 g
Dimensions 126.00 × 93.00 × 112.00 mm