Rutile blue red-brown stoneware mug

$35.00

Rutile blue red-brown stoneware mug

SKU: AJ24075 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24075
Run/Test Number: P6850
Technique: Hand-rolled, embossed and assembled, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze Inside – L3500G+2Fe
Glaze Outside – GA6-C+2% iron oxide
Clay BodyM390
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 97 mm (3.8 in)
Depth at rim (including handle) – 134 mm (5.3 in)
Height – 101 mm (4.0 in)
Weight – 353 grams (12.4 oz)

Registration Page: https://digitalfire.com/potterytony/2415

Weight 353 g
Dimensions 134.00 × 97.00 × 101.00 mm