Bamboo tan incised stoneware mug

$30.00

Bamboo tan incised stoneware mug

SKU: AJ24149 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24149
Run/Test Number: L4062A
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideG2571A
Glaze OutsideG2571A
EngobeL3954N
Clay Body – B-Mix
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 105 mm (4.1 in)
Depth at rim (including handle) – 136 mm (5.4 in)
Height – 91 mm (3.6 in)
Weight – 382 grams (13.5 oz)

Registration Page: https://digitalfire.com/potterytony/2345

Weight 382 g
Dimensions 136.00 × 105.00 × 91.00 mm