Red folded Polar Ice porcelain mug

$30.00

Red folded Polar Ice porcelain mug

SKU: AJ24085 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24085
Run/Test Number: P6845
Technique: Hand-assembled, pour-glazed inside, waxed, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideG2934Y Red
Clay BodyPolar Ice
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 96 mm (3.8 in)
Depth at rim (including handle) – 121 mm (4.8 in)
Height – 100 mm (3.9 in)
Weight – 297 grams (10.5 oz)

Registration Page: https://digitalfire.com/potterytony/2425

Weight 297 g
Dimensions 121.00 × 96.00 × 100.00 mm