For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24074
Run/Test Number: L4283
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.
Firing Schedule – C6DHSC
Temperature – Cone 6
Glaze Inside – G2926B
Glaze Outside – GA6-B
Clay Body – L4283 MNP
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 88 mm (3.5 in)
Depth at rim (including handle) – 117 mm (4.6 in)
Height – 100 mm (3.9 in)
Weight – 313 grams (11.0 oz)
Registration Page: https://digitalfire.com/potterytony/2410