Bamboo tan incised stoneware mug

$35.00

Bamboo tan incised stoneware mug

SKU: AJ24320 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24320
Run/Test Number: P6902
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideGR10-C
Glaze OutsideG2571B
EngobeL3954N
Clay Body – H450
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 97 mm (3.8 in)
Depth at rim (including handle) – 127 mm (5.0 in)
Height – 115 mm (4.5 in)
Weight – 393 grams (13.9 oz)

Registration Page: https://digitalfire.com/potterytony/2465

Weight 393 g
Dimensions 127.00 × 97.00 × 115.00 mm