Glossy jet black porcelain mug

$40.00

Glossy jet black porcelain mug

SKU: AJ24315 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24315
Run/Test Number: P6932
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideG3914A
Glaze OutsideG2926BL
Clay BodyM370
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 100 mm (3.9 in)
Depth at rim (including handle) – 130 mm (5.1 in)
Height – 118 mm (4.6 in)
Weight – 343 grams (12.1 oz)

Registration Page: https://digitalfire.com/potterytony/2460