Variegated glossy blue mug

$35.00

Variegated glossy blue mug

SKU: AJ24104 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24104
Run/Test Number: P6768
Technique: Thrown, incised, dip-glazed

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideGR6-M
Glaze Outside – GR6-M
Clay BodyM332
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 102 mm (4.0 in)
Depth at rim (including handle) – 133 mm (5.2 in)
Height – 124 mm (4.9 in)
Weight – 469 grams (16.5 oz)

Registration Page: https://digitalfire.com/potterytony/2446

Weight 469 g
Dimensions 133.00 × 102.00 × 124.00 mm