Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideGA6-C
Glaze Outside – GA6-C
EngobeL3954B
Clay BodyM340
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 107 mm (4.2 in)
Depth at rim (including handle) – 138 mm (5.4 in)
Height – 109 mm (4.3 in)
Weight – 526 grams (18.5 oz)