Deep blue matte stoneware mug

$35.00

This H550 compatible clay body is made from Flintoft, Saskatchewan ball clay and Plainsman 3D.

SKU: AJ24336 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24336
Run/Test Number: L4382A
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed
Description: This H550 compatible clay body is made from Flintoft, Saskatchewan ball clay and Plainsman 3D.

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideG2571F
Glaze OutsideG2571F blue MgO matte
EngobeL3954N
Clay BodyH550 test
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 98 mm (3.9 in)
Depth at rim (including handle) – 130 mm (5.1 in)
Height – 106 mm (4.2 in)
Weight – 341 grams (12.0 oz)

Registration Page: https://digitalfire.com/potterytony/2479

Weight 341 g
Dimensions 130.00 × 98.00 × 106.00 mm