Run/Test Number: L4484D
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideG3914A
Glaze OutsideG3939A
Clay BodyL4484D MNP black
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 97 mm (3.8 in)
Depth at rim (including handle) – 130 mm (5.1 in)
Height – 116 mm (4.6 in)
Weight – 358 grams (12.6 oz)

Registration Page: https://digitalfire.com/potterytony/2502

Weight 358 g
Dimensions 130.00 × 97.00 × 116.00 mm