Floating-blue stoneware mug

$35.00

Floating-blue stoneware mug

SKU: AJ24361 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24361
Run/Test Number: L4471D
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideGR6-M
Glaze Outside – PLC6DS
Clay BodyM390 test
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 95 mm (3.7 in)
Depth at rim (including handle) – 128 mm (5.0 in)
Height – 109 mm (4.3 in)
Weight – 348 grams (12.3 oz)

Registration Page: https://digitalfire.com/potterytony/2503