For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24363
Run/Test Number: L4471G
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – PLC6DS
Temperature – Cone 6
Glaze Inside – GA6-B
Glaze Outside – GR6-M
Clay Body – M390 test
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 95 mm (3.7 in)
Depth at rim (including handle) – 130 mm (5.1 in)
Height – 123 mm (4.8 in)
Weight – 369 grams (13.0 oz)
Registration Page: https://digitalfire.com/potterytony/2505