Deep blue matte stoneware mug

$35.00

This H550 compatible clay body is made from Flintoft, Saskatchewan ball clay and Plainsman 3D.

SKU: AJ24338 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24338
Run/Test Number: L4376A
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed
Description: This H550 compatible clay body is made from Flintoft, Saskatchewan ball clay and Plainsman 3D.

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideG2571F
Glaze OutsideG2571F blue MgO matte
EngobeL3954N
Clay BodyH550 Test
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 97 mm (3.8 in)
Depth at rim (including handle) – 129 mm (5.1 in)
Height – 109 mm (4.3 in)
Weight – 353 grams (12.4 oz)

Registration Page: https://digitalfire.com/potterytony/2480

Weight 353 g
Dimensions 129.00 × 97.00 × 109.00 mm