Bamboo tan incised stoneware mug

$30.00

H550 compatible clay body made from Blue Hills, Saskatchewan ball clay and Plainsman 3D.

SKU: AJ24354 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24354
Run/Test Number: L4377C
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside
Description: H550 compatible clay body made from Blue Hills, Saskatchewan ball clay and Plainsman 3D.

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideGR10-C
Glaze OutsideG2571B bamboo matte
EngobeL3954N
Clay BodyH550
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 94 mm (3.7 in)
Depth at rim (including handle) – 127 mm (5.0 in)
Height – 97 mm (3.8 in)
Weight – 348 grams (12.3 oz)

Registration Page: https://digitalfire.com/potterytony/2493

Weight 348 g
Dimensions 127.00 × 94.00 × 97.00 mm