Run/Test Number: L4486B
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG3914A
Glaze OutsideGR6-M
Clay Body – L4486B MNP
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 96 mm (3.8 in)
Depth at rim (including handle) – 131 mm (5.2 in)
Height – 111 mm (4.4 in)
Weight – 339 grams (11.9 oz)

Registration Page: https://digitalfire.com/potterytony/2519