Zero4 fritware porcelain hash-tag mug

$50.00

Zero4 fritware porcelain hash-tag mug

SKU: AJ24404 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24404
Run/Test Number: L3924J
Technique: Thrown, leather-hard under-glaze decorated, incised, 1650F bisque fired, dip-glazed

Firing ScheduleC04PLTP
TemperatureCone 04
Glaze InsideG3879C
Glaze OutsideG3879C
Clay BodyL3924J
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 97 mm (3.8 in)
Depth at rim (including handle) – 129 mm (5.1 in)
Height – 135 mm (5.3 in)
Weight – 400 grams (14.1 oz)

Registration Page: https://digitalfire.com/potterytony/2533

Weight 400 g
Dimensions 129.00 × 97.00 × 135.00 mm