Bamboo tan incised stoneware mug

$40.00

Bamboo tan incised stoneware mug

SKU: AJ24411 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24411
Run/Test Number: L4040A
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideGR10-C
Glaze OutsideG2571A Bamboo
EngobeL3954N
Clay BodyH555
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 99 mm (3.9 in)
Depth at rim (including handle) – 129 mm (5.1 in)
Height – 104 mm (4.1 in)
Weight – 357 grams (12.6 oz)

Registration Page: https://digitalfire.com/potterytony/2546

Weight 357 g