Bamboo tan incised stoneware mug

$40.00

Bamboo tan incised stoneware mug

SKU: AJ24396 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24396
Run/Test Number: P6679
Technique: Hand-rolled and assembled, engobed inside and top outside, incised, dip-glazed

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideG2571A Bamboo
Glaze OutsideG2571A Bamboo
EngobeL3954N
Clay BodyH550
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 97 mm (3.8 in)
Depth at rim (including handle) – 132 mm (5.2 in)
Height – 107 mm (4.2 in)
Weight – 306 grams (10.8 oz)

Registration Page: https://digitalfire.com/potterytony/2542

Weight 306 g
Dimensions 132.00 × 97.00 × 107.00 mm