Red and black Polar Ice porcelain mug

$40.00

Red and black Polar Ice porcelain mug

SKU: AJ24427 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24427
Run/Test Number: P7027
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG3914A
Glaze OutsideG2934Y Red
Clay BodyM370
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 93 mm (3.7 in)
Depth at rim (including handle) – 122 mm (4.8 in)
Height – 113 mm (4.4 in)
Weight – 356 grams (12.5 oz)

Registration Page: https://digitalfire.com/potterytony/2560

Weight 356 g
Dimensions 122.00 × 93.00 × 113.00 mm