Serial Number: AJ24437
Run/Test Number: P7027
Technique: Thrown, liner-glazed inside, dip-glazed outside
Firing Schedule – C6DHSC
Temperature – Cone 6
Glaze Inside – G2926BL
Glaze Outside – G2934Y Black
Engobe – L3954B
Clay Body – M370
Foot Style – Unglazed flat black engobed
Width at rim (perpendicular to handle) – 93 mm (3.7 in)
Depth at rim (including handle) – 125 mm (4.9 in)
Height – 111 mm (4.4 in)
Weight – 393 grams (13.9 oz)
Registration Page: https://digitalfire.com/potterytony/2570