For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24367
Run/Test Number: P6967
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – PLC6DS
Temperature – Cone 6
Glaze Inside – G2926B
Glaze Outside – G2934Y blue
Clay Body – Polar Ice
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 93 mm (3.7 in)
Depth at rim (including handle) – 126 mm (5.0 in)
Height – 118 mm (4.6 in)
Weight – 389 grams (13.7 oz)
Registration Page: https://digitalfire.com/potterytony/2509