Bamboo tan incised stoneware mug

$30.00

Bamboo tan incised stoneware mug

SKU: AJ24151 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24151
Run/Test Number: BMix
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideGR10-C
Glaze OutsideG2571A
EngobeL3954N
Clay Body – B-Mix 10
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 108 mm (4.3 in)
Depth at rim (including handle) – 136 mm (5.4 in)
Height – 122 mm (4.8 in)
Weight – 381 grams (13.4 oz)

Registration Page: https://digitalfire.com/potterytony/2346

Weight 381 g
Dimensions 136.00 × 108.00 × 122.00 mm